Parameter | Symbol | Min | Max | Unit | Condition |
Operating Case Temperature | Tc | -20 | 70 | °C | -- |
Storage Temperature | Tstg | -40 | 85 | °C | -- |
Reverse Voltage | Vr | -- | 3 | V | -- |
Forward current | I | -- | 1000 | mA | -- |
Thermoelectric cooler voltage | VTEC | -- | 2.6 | V | -- |
Thermoelectric cooler current | ITEC | -- | 1.5 | A | -- |
Lead solder Temperature | -- | -- | 260 | °C | -- |
Lead Soldering Time | -- | -- | 10 | s | -- |
Parameter | Symbol | Min | Typ | Max | Unit | Test Conditions |
Pulse power | Po | - | - | 150 | mW | T=25ºC |
Pulse current | I | - | - | 1000 | mA | T=25ºC |
Pulse width | S | - | 10 | - | us | T=25ºC |
Duty cycle | % | - | 1% | - | - | T=25ºC |
Voltage | Vop | - | - | 2.5 | V | T=25ºC |
Operating wavelength (optional FP) | λC | 1540 | 1550 | 1560 | nm | T=25ºC |
Edge touch rejection ratio (optional FP) | SMSR | 35 | 45 | - | dB | T=25ºC |
Thermistor | Rth | 9.5 | 10 | 10.5 | KΩ | T=25ºC |
Optical Isolation (Optional) | - | 35 | - | - | dB | T=25ºC |
RZLD | wavelength | Output Power | encapsulation &Fiber selection | Connector | PIN |
RZLD=LD | …nm | …mW | BP=BTF PM Fiber | 00=NO | 14 |
RZSLD=SLED | 974 | 5 | BS=BTF SM Fiber | FA=FC/APC | 10 |
RZNLD=Narrow line width | 1064 | 50 | BM=BTF MM Fiber | FU=FC/UPC | 8 |
RZPLD= Pulsed laser | 1310 | 200 | DP=DIP PM Fiber | SA=SC/APC | 6 |
RZSOA=SOA … |
1550 … |
400 … |
… | … |